K11防水涂料由优质的水泥细砂及独特的非常活跃的高分子聚合物组成。它与K11添加按一
定比例混合以后,能极大地改善胶浆的粘结力、保水性和柔韧性,同时提高了防水层的耐磨性能,干固后不会产生收缩,并且可
以抑制霉菌的生长和防水盐份的污染。
 
产品特点
1  具有一定的柔韧性,能够覆盖头发丝般的裂缝(小于0.4mm)以及抵御轻微的震动。
2、能在潮湿的环境下施工。
3、具有较好的抗弯、抗折、耐老化性能。
4、无毒无害,环保产品。
Features
1.      flexible to some extent, be able to cover crack as small as hair(less than 0.4mm) and resist light shock.
2.   Construct under damp environment;
3.   good resistance to bending, resistance to break and resistance to aging.
4. . No toxicity, no nocuity its a new eco-friendly product.
 
 
适用范围
1、室内外混凝土结构、水泥抹底、轻质砖墙等。
2、基面的建筑物地基、屋顶、地下室、隧道、矿井、水槽防水工程等。
Applications:
1.      concrete structure of inner and outer house, base of cement, light brick wall.
2.      base plane of building base, roofing, basement, tunnel, mine and water channel.
 
基面处理
1、基层表面应密实、平整、干燥、无裂缝、无油污、灰尘等附着物。
2、小空隙,砂眼须用水泥砂浆抹平,尖锐的边缘应除去。
3、涂抹浆料之前,应充分润湿底材,但不能有积水。
Base plane process:
1.      Keep the surface plane, solid, clean without oil dirt, dust or other loose matters
2.      gap and hole should be filled by cement mortar and sharp edges must be eliminated
3.      . Wet the base material till no seeable water
 
施工工艺
1、先将液料倒入容器,再将粉料慢慢倒入其中,充分搅拌至均匀无颗粒、无沉淀的膏糊状,静置五分钟后,再搅拌一次,使
  用效果更佳。
2、用毛刷或滚刷直接涂刷胶浆于基面上,不可漏刷,为防止沉淀,操作过程中应保持间断性搅拌。
4、一般涂刷两遍以上(各涂层的方向应该交错),最后的涂膜厚度保持在1.2-1.4mm,用量约为2.5kg/m2
5、浆料涂刷第二天起,建议用细雾喷水或湿布覆盖涂层2-3天,如长期盛水的水池应待其空置两周后才盛水,热水或腐蚀性液体
  池则需要空置三周时间。
Technical process
1.      pour the liquid into the container and fully stir until turn to be cream with no granules and no deposit , stir again after 5 minutes to make it better.
2. Use brush or rolling brush to coat the paint on the base surface, keep stirring in a interval to avoid depositing;
3.  Two times of brushing is needed (two directions), the final coating film should have 1.2-1.4mm depth, 2.5kg/m2;
4.   from the second day of painting, should use mist to water it or wet cloth to cover for 2-3 days, If for pool always with water, should pour water, hot water or corrosive liquid into it after two weeksvacancy .
     Pool need to be vacant for three weeks.
 
 
注意事项
1  施工中应保证本品完全覆盖基面,防水层完全干固后方可做其它作业。
2、浆料涂后24小时之内,需采取保护措施以防止踩踏、雨水、霜冻、烈日暴晒等对涂层造成的损害。
3、不能在0以下施工,不要在特别潮湿又不通风的环境中施工。
4、切忌将已干结的胶浆加水混合后再用。
Cautions:
1.Ensure the base material is fully covered and other works could be conducted in 24 hours
2.measures should be taken to prevent from being stamping, rain, frost, burning sun within 24 hours.
3.no construction below 0℃and in moist and airlessenvironment
4.Do NOT add water into the dried mortar for second use.
 
包装储存
置于阴凉干燥处,未开封的本品可贮存12个月。
Packaging and storage
Keep it in shade and dry place, storage life is 12 months if unsealed.
本条信息网址: https://www.fa08.com.cn/gongying/show-492504.html
免责声明: 本网站内容来源于网友提供和互联网公开资料等,仅供参考。本网站不对网站所有信息的准确性、可靠性或完整性提供任何保证,交易汇款需谨慎,请注意调查核实。若文中涉及有违公德、触犯法律的内容,一经发现,立即删除,作者需自行承担相应责任。涉及到版权或其他问题,请及时联系,我们将在收到通知后第一时间妥善处理。
0条 [查看全部]  相关评论
 
更多»本企业其它产品

[ 供应信息搜索 ]  [ 加入收藏 ]  [ 告诉好友 ]  [ 打印本文 ]  [ 违规举报 ]  [ 关闭窗口 ]

 
网站首页 | 关于我们 | 联系方式 | 常见问题 | sitemaps | 网站地图 | 排名推广 | 广告服务 | 积分换礼 | 网站留言 | RSS订阅|
行业图标
免费发布信息,上网做生意,就上发吧信息网.发吧,发吧,祝您生意发发!(c)2008-2021 DESTOON B2B SYSTEM All Rights Reserved
本站内容系用户自行发布,其真实性、合法性由发布人负责,发吧信息网(www.fa08.com.cn)不提供任何保证,亦不承担任何法律责任